Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00094 cm/cm
0.00094 in/in
ASTM D955
Plenco 7556 Phenolic, Briquette, Transfer Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..