Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00071 cm/cm | 0.00071 in/in | Cold Part VS Cold Tool; ASTM D955 |
Applied Composites 120 Polyester SMC Industry Application: ElectricalProduct Application: Transmission ProductDistinct Features: Pigmentable UL 94 V-5, Stable @ 600 Hour QUV Accelerated Weather Testing, Passed 6 Mos. AZ Outdoor Weather.. |