Polymer Property : Linear Mold Shrinkage = 0.00025 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00025 cm/cm
0.00025 in/in
Polymerization Shrinkage
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC
Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st..
Linear Mold Shrinkage 0.00025 cm/cm
0.00025 in/in
Polymerization Shrinkage
Premix Premi-Glas® 1206 LD Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1206 LD is a fiberglass reinforced thermoset sheet molding compound for transportation or structural and semi-structural applications where good surface appearance, high strength and du..
Linear Mold Shrinkage 0.00025 cm/cm
0.00025 in/in
Polymerization Shrinkage
Premix Premi-Glas® 2550® AM CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas 2550® AM CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generati..
Linear Mold Shrinkage 0.00025 cm/cm
0.00025 in/in
Polymerization Shrinkage
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation ..