Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 100 hour | 100 hour | F50; ASTM D1693 |
ICO Polymers ICORENEâ„¢ 190-3561 LMDPE Rotational Molding Resin Description: ICORENE 190-1332 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Ke.. |
|||
ESCR 10% Igepal® | 100 hour | 100 hour | F50; ASTM D1693 |
ICO Polymers ICORENEâ„¢ 195-1326 LMDPE Rotational Molding Resin Description: ICORENE 195-1326 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Ke.. |
|||
ESCR 10% Igepal® | 100 hour | 100 hour | F50; ASTM D1693 |
ICO Polymers ICORENEâ„¢ 195-4060 LMDPE Rotational Molding Resin Description: ICORENE 195-4060 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |