Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Permeability | 7.10 g mil/ (m2 day) @Temperature 37.8 °C |
0.458 g mil/ (100 in2 day) @Temperature 100 °F |
90% RH; ASTM E96 |
Total PPH 3230 Polypropylene, Blow Molding Grade Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optim.. |
|||
Water Vapor Permeability | 7.10 g mil/ (m2 day) @Temperature 37.8 °C |
0.458 g mil/ (100 in2 day) @Temperature 100 °F |
90% RH; ASTM E96 |
Total PPR 3230XZ Polypropylene, Blow Molding Grade Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac.. |