Polymer Property : Water Vapor Permeability = 0.0635 g mil/ (100 in2 day) Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Permeability 0.985 g mil/ (m2 day)
0.0635 g mil/ (100 in2 day)
Topas Advanced Polymers TOPAS® 8007D-61 Cyclic Olefin Copolymer (COC)
TOPAS® 8007D-61 is an externally lubricated version of our 8007 series of injection molding resins, targeting injection blow molding (IBM) and injection stretch blow molding (ISBM) applications. Li..