Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 7700 dtex | 6930 denier | |
Toho Tenax Besfight® G50-300 12K HMA-7C EP01 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |