Polymer Property : Fiber Count = 670 denier Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 744 dtex
670 denier
Shakespeare Resistat® F9216 F040 Nylon 66 Monofilament
Resistat F2416, MERGE F040 is a nylon 6,6 multifilament yarn. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section with a coating th..
Fiber Count 744 dtex
670 denier
Shakespeare Resistat® F9416 M040 Nylon 66 Monofilament
Resistat F9416, MERGE M040 is composed of forty filaments of conductive nylon 6,6 yarn. This yarn is twisted and heatset. Each filament has electrically conductive carbon suffused into the surface..