Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 583 dtex | 525 denier | |
Shakespeare ISOray Fluoropolymer UV resistant sewing thread, diameter 0.008" Extreme UV resistant, highly transparent, fluoropolymer monofilament industrial sewing thread. Excellent chemical resistance, excellent soil release and low moisture regain. Used for sewing: Awnin.. |