Physical Properties Metric English Comments
Fiber Count 455.9 - 484.1 dtex
410.3 - 435.7 denier
Voloknohim Filament Nylon Linear Density 47 tex
Application: for production of goods for fishery and for other technical purposes. The produced yarn is bright, UV-stabilized, thermostabilized, UV-thermostabilized, not dyed, dyedInformation provi..