Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 37400 dtex | 33700 denier | |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5.5, Diameter 2 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |