Polymer Property : Fiber Count = 36500 denier Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 40600 dtex
36500 denier
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=6)
Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE.