Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 3940 dtex | 3550 denier | |
Toho Tenax Besfight® G60-600 12K UMA-5C A303 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |