Polymer Property : Fiber Count = 3330 dtex Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 3330 dtex
3000 denier
roving
3M Nextel™ XN-625 Woven Fabric 720
Information provided by 3M
Fiber Count 3330 dtex
3000 denier
roving
3M Nextel™ DF-19 Woven Fabric 610
Information provided by 3M