Physical Properties Metric English Comments
Fiber Count 36400 dtex
32800 denier
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=4.5, Diameter 2 mm)
Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic..