Polymer Property : Fiber Count = 3240 denier Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 3600 dtex
3240 denier
Toho Tenax Besfight® MC Type I (3000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..