Physical Properties Metric English Comments
Fiber Count 3.10 - 4.20 dtex
2.79 - 3.78 denier
EMS-Griltech Grilon® TM 5000 White Nylon 6 Fiber, Low Fiber Count
Description: GRILON TM 5000 is a standard product for the manufacturing of press felts. This is a technical fiber with medium-set fixation. This fiber is also available as TM 5010 (low crimp) and TM..
Fiber Count 3.30 - 4.20 dtex
2.97 - 3.78 denier
EMS-Griltech Grilon® M 369 White Nylon 6 Fiber
Description: GRILON M 369 is a fine PA6 fiber with soft interlinings for special thermobonding properties and low shrinkage in the soft end product. The coarser counts, 3.3 - 4.2 dtex, are also used..