Physical Properties Metric English Comments
Fiber Count 2020 dtex
1820 denier
Toho Tenax Besfight® G30-500 3K HTA-7C EP01 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Fiber Count 2020 dtex
1820 denier
Toho Tenax Besfight® G30-500 3K HTA-7C EP03 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Fiber Count 2020 dtex
1820 denier
Toho Tenax Besfight® G30-500 3K HTA-7W EP01 Continuous Filament Carbon Fiber
Standard Modulus; Twisted; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon..