Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 1800 dtex | 1620 denier | |
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance .. |