Polymer Property : Fiber Count = 1600 denier Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 1780 dtex
1600 denier
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber
Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (..