Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 178 dtex | 160 denier | |
Shakespeare WonderThread® M-7 diameter 0.005" Polyester Industrial Sewing Thread Applications: Specialty industrial sewing applications demanding polyester for:
1) Certifications that sewn goods are 100% polyester Chemical Resistance-polyester withstands low Ph, acidic enviro.. |