Polymer Property : Fiber Count = 15.3 denier Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 17.0 - 100 dtex
15.3 - 90.0 denier
EMS-Griltech Grilon® TM 5000 White Nylon 6 Fiber, High Fiber Count
Description: GRILON TM 5000 is a standard product for the manufacturing of press felts. This is a technical fiber with medium-set fixation. This fiber is also available as TM 5010 (low crimp) and TM..
Fiber Count 17.0 - 22.0 dtex
15.3 - 19.8 denier
EMS-Griltech Grilon® TN 2200 White Nylon 6 Fiber
Description: GRILON TN 2200 is used for woolen yarns which is then further processed to produce technical fabrics.Applications: Press Felt FabricData provided by EMS-Griltech.
Fiber Count 17.0 - 30.0 dtex
15.3 - 27.0 denier
EMS-Griltech Grilon® BA 140 White Nylon 66/CoPA Bi-Component Fiber
Description: GRILON BA 140 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 135 - 145 °C. The fine count bi-component fiber guarantees an even distrib..