Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 1490 dtex | 1340 denier | |
UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.8) Specialties: Medium viscosity Nylon 6/66 Copolymer, High knot strength (for Knot improvement), Softness is similar with 1022MT2 (At the heat setting of the net, higher shrink ratio may be expected t.. |
|||
Fiber Count | 1490 dtex | 1340 denier | |
UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=5) Specialties: Medium viscosity Nylon 6/66 Copolymer, High knot strength (for Knot improvement), Softness is similar with 1022MT2 (At the heat setting of the net, higher shrink ratio may be expected t.. |
|||
Fiber Count | 1490 dtex | 1340 denier | |
UBE 5033T Nylon 6/66 Monofilament (Drawing Ratio=5.5) Specialties: High viscosity Nylon 6/66 Copolymer, High transparent and tenacity, Higher drawing ratio can be achieved for superior line strengthApplications: Small-medium size sport fishing line Inf.. |