Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 1360 dtex | 1220 denier | Per Filament |
Shakespeare Sanstat® CN125 .36mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |