Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 1480 dtex | 1330 denier | Per Filament |
Shakespeare Sanstat® CN125 .41mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |
|||
Fiber Count | 1480 dtex | 1330 denier | |
UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.5) Specialties: Medium viscosity Nylon 6/66 Copolymer, High knot strength (for Knot improvement), Softness is similar with 1022MT2 (At the heat setting of the net, higher shrink ratio may be expected t.. |
|||
Fiber Count | 1480 dtex | 1330 denier | |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5, Diameter 0.4 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |