Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.410 - 0.410 cc-mm/m²-24hr-atm @Temperature 37.8 - 37.8 °C |
1.04 - 1.04 cc-mil/100 in²-24hr-atm @Temperature 100 - 100 °F |
Average value: 0.410 cc-mm/m²-24hr-atm Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Moisture Vapor Transmission | 0.410 - 0.410 cc-mm/m²-24hr-atm @Thickness 0.0254 - 0.0254 mm |
1.04 - 1.04 cc-mil/100 in²-24hr-atm @Thickness 0.00100 - 0.00100 in |
Average value: 0.410 cc-mm/m²-24hr-atm Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |