Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 4320 hour @Temperature 24.0 °C |
4320 hour @Temperature 75.2 °F |
No Failure; HIP+HT; Rockwell Hardness C - 40; Test Type - C-Ring; Test Condition - 25% NaCl in H<sub>2</sub>O + a gas mixture of 15% H<sub>2</sub>S, 15% CO<sub>2</sub> and 70% N<sub>2</sub> coupled to carbo |
Crucible Compaction Metals P/M 625M Corrosion Resistant Alloy P/M 625M (chemically, UNS N07626) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The a.. |