Physical Properties Metric English Comments
Environmental Stress Crack Resistance >= 1200 hour

@Temperature 50.0 °C
>= 1200 hour

@Temperature 122 °F
F 0 (25% Igepal); ASTM D1693
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin  (discontinued **)
Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by..