Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR, Bottle | 55 hour @Temperature 23.0 °C |
55 hour @Temperature 73.4 °F |
F<sub>50</sub>; ASTM D1693 |
SIDPEC EGYPTENE® HD 6070 UA HDPE Injection Molding Applications:CratesBoxesSeatsPalletsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |