Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LB5604 High Density Polyethylene ApplicationsThe PETROTHENE LB 5604 series of polyethylene resins exhibits good stiffness and environmental stress cracking resistance. Typical applications include household chemical and person car.. |
|||
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Regulatory StatusThe base resin LR 7320 meets t.. |
|||
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR732013 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
ESCR, Bottle | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |