Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR, Bottle | 150 hour @Temperature 60.0 °C |
150 hour @Temperature 140 °F |
F<sub>50</sub> |
Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer