Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 0.700 - 3.50 g/10 min | 0.700 - 3.50 g/10 min | Average value: 1.71 g/10 min Grade Count:16 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |