Polymer Property : Base Resin Melt Index = 1.3 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Base Resin Melt Index 1.3 g/10 min
1.3 g/10 min
ASTM D1238
Eastman E6838-902F Polyethylene Film  (discontinued **)
Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business ..