Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 0.75 g/10 min | 0.75 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |