Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANLENE® LDF264YZ Low density polyethylene LDF264YZ is a low density polyethylene resin for film extrusion. LDF264YZ has no slip and anti-block additives. LDF264YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |