Polymer Property : Base Resin Melt Index = 0.33 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Base Resin Melt Index 0.33 g/10 min
0.33 g/10 min
ASTM D1238
Lotte Chemical Titan TITANLENE® LDF265YZ Low density polyethylene
LDF265YZ is a low density polyethylene resin for film extrusion. LDF265YZ has no slip and anti-block additives. LDF265YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..