Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene HI2200 is a high density polyethylene for injection molding. HI2200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Ap.. |
|||
Base Resin Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |