Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci.. |