Polymer Property : Antiblock Level = 8000 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Antiblock Level 8000 ppm
8000 ppm
ExxonMobil NTX™ NTX 095 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
Antiblock Level 8000 ppm
8000 ppm
ExxonMobil NTX™ NTX 150 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..