Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 6900 ppm | 6900 ppm | |
Formosa Plastics Formolene® L62608PE Film (Hexene Grade) LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |