Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 6500 ppm | 6500 ppm | |
ExxonMobil NTX™ NTX 104 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Antiblock Level | 6500 ppm | 6500 ppm | |
ExxonMobil NTX™ NTX 141 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |