Polymer Property : Antiblock Level = 5050 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Antiblock Level 5050 ppm
5050 ppm
ExxonMobil LD 307.76 Clear, High Impact Film Resin
LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical