Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 2900 ppm | 2900 ppm | |
Dow 751A Low Density Polyethylene Resin A high additive film resin for general packaging applications For cast film extrusion A fast blooming resin for high speed bag conversion Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information p.. |