Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 25 ppm | 25 ppm | modified ASTM D-5630 |
Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch
(discontinued **) Metallocene polyethylene antiblock masterbatch. This antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require: Reduced COFMinim.. |
|||
Antiblock Level | 25 ppm | 25 ppm | modified ASTM D-5630 |
Chevron Phillips MarFlex® ER3344 Polyethylene; Masterbatch
(discontinued **) Metallocene polyethylene antiblock masterbatch. This erucamide slip and antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require.. |