Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 1700 ppm | 1700 ppm | |
Formosa Plastics Formolene® L42009PE Film (Butene Grade) LLDPE Linear Low Density Polyethylene Butene Copolymer for Film Extrusion Formolene® L42009PE is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excell.. |
|||
Antiblock Level | 1700 ppm | 1700 ppm | |