Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 15000 ppm | 15000 ppm | |
LyondellBasell Ultrathene® UE672317 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |