Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 1400 ppm | 1400 ppm | |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |