Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 10000 ppm | 10000 ppm | |
Chevron Phillips MarFlex® 5429 Low Density Polyethylene, Cast Film This LDPE is tailored for cast film applications that require:Excellent openabilitySuited for high speed convertingGood clarityMedium coefficient of frictionTypical cast film applications include:Co.. |
|||
Antiblock Level | 10000 ppm | 10000 ppm | |
ExxonMobil Escorene® LD 720.01 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |