Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 833 ppm | 833 ppm | |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |