Physical Properties Metric English Comments
Slip Level 1700 ppm
1700 ppm
ExxonMobil LL 1002x74 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Slip Level 1700 ppm
1700 ppm
ExxonMobil LL 1002x79 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Slip Level 1700 ppm
1700 ppm
ExxonMobil LL 1001x74 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Slip Level 1700 ppm
1700 ppm
ExxonMobil LL 1107x95 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Slip Level 1700 ppm
1700 ppm
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Slip Level 1700 ppm
1700 ppm
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin